L450-PSL1 Chemische samenstelling (%)
| samenstelling | C | Mn | P | S | Cr | Ni | Cu | ma | B | Meer | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Naadloze pijp | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti Kleiner dan of gelijk aan 0.15 |
| Max | 0.28 | 1.4 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
| samenstelling | C | Mn | P | S | Cr | Ni | Cu | ma | B | Meer | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Gelaste pijp | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti Kleiner dan of gelijk aan 0.15 |
| Max | 0.26 | 1.45 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
L450-PSL1 Mechanische eigenschappen
| Type | Treksterkte σb Mpa |
Opbrengstpunt σs Mpa |
Rek bij breuk of rek δ % |
|---|---|---|---|
| Naadloos/gelast | Groter dan of gelijk aan 535 | Groter dan of gelijk aan 450 |
L450Q-PSL2 Chemische samenstelling (%)
| samenstelling | C | Si | Mn | P | S | Cr | Ni | Cu | ma | B | Meer | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Naadloze/gelaste buis | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti Kleiner dan of gelijk aan 0.15 |
| Max | 0.18 | 0.45 | 1.7 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |
L450Q-PSL2 Mechanische eigenschappen
| Type | Testtemperatuur | Treksterkte σb Mpa |
Opbrengstpunt σs |
Rek bij breuk of rek δ |
Schok geabsorbeerde energie |
|---|---|---|---|---|---|
| Naadloos/gelast | 535~760 | 450~600 | |||
| OD Kleiner dan of gelijk aan 30 | 0 graad | Groter dan of gelijk aan 27 | |||
| OD>30~48 | 0 graad | Groter dan of gelijk aan 40 | |||
| OD>48~84 | 0 graad | Groter dan of gelijk aan 54 |
L450M-PSL2 Chemische samenstelling (%)
| Samenstelling | C | Si | Mn | P | S | Cr | Ni | Cu | ma | B | Meer | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Gelast | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti Kleiner dan of gelijk aan 0.15 |
| Max | 0.18 | 0.45 | 1.6 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |
GNEE API L450 pijpleiding te koop