API 5DP boorpijpgroottesbereik
Bereik van maten: 2 3/8 "tot 5 1/2"
Bereik van dikte: 6,5 mm tot 12,7 mm
Lengte: R1, R2, R3
|
Grootte OD |
Nominaal |
Het gewicht berekenen |
Cijfer |
Dikte |
Verdikte vorm (zie opmerking) |
|||
|
in. |
mm |
lb/ft |
kg/m |
in. |
mm |
|||
|
2 3/8 |
60.3 |
6.65 |
6.26 |
9.32 |
E,X,G,S |
0.280 |
7.11 |
EU |
|
2 7/8 |
73.0 |
10.4 |
9.72 |
14.48 |
E,X,G,S |
0.362 |
9.19 |
Eu, iu |
|
3 1/2 |
88.9 |
9.50 |
8.81 |
13.12 |
E |
0.254 |
6.45 |
Eu, iu |
|
3 1/2 |
88.9 |
13.30 |
12.31 |
18.34 |
E,X,G,S |
0.368 |
9.35 |
Eu, iu |
|
3 1/2 |
88.9 |
15.50 |
14.63 |
21.79 |
E |
0.449 |
11.40 |
Eu, iu |
|
3 1/2 |
88.9 |
15.50 |
14.63 |
21.79 |
X,G,S |
0.449 |
11.40 |
EU, IEU |
|
4 |
101.6 |
14.00 |
12.93 |
19.26 |
E,X,G,S |
0.330 |
8.38 |
Eu, iu |
|
4 1/2 |
114.3 |
13.75 |
12.24 |
18.23 |
E |
0.271 |
6.88 |
Eu, iu |
|
4 1/2 |
114.3 |
16.60 |
14.98 |
22.31 |
E,X,G,S |
0.337 |
8.56 |
EU, IEU |
|
4 1/2 |
114.3 |
20.00 |
18.69 |
27.84 |
E,X,G,S |
0.430 |
10.92 |
EU, IEU |
|
5 |
127.0 |
16.25 |
14.87 |
22.15 |
X,G,S |
0.296 |
7.52 |
IU |
|
5 |
127.0 |
19.50 |
17.93 |
26.71 |
E |
0.362 |
9.19 |
IEU |
|
5 |
127.0 |
19.50 |
17.93 |
26.71 |
X,G,S |
0.362 |
9.19 |
EU, IEU |
|
5 |
127.0 |
25.60 |
24.03 |
35.79 |
E |
0.500 |
12.70 |
IEU |
|
5 |
127.0 |
25.60 |
24.03 |
35.79 |
X,G,S |
0.500 |
12.70 |
EU, IEU |
|
5 1/2 |
139.7 |
21.90 |
19.81 |
29.51 |
E,X,G,S |
0.361 |
9.17 |
IEU |
|
5 1/2 |
139.7 |
24.70 |
22.54 |
33.57 |
E,X,G,S |
0.415 |
10.54 |
IEU |